Steel parts repair in our Colorado shop

Cracked brackets, bent guards and broken mounts brought to our shop, repaired, and where it makes sense, reinforced so the same crack does not come back.

Cracked rusty steel bracket beside the same bracket repaired with a smooth weld and a new gusset

How we approach steel parts repair

A part that cracked once will usually crack again in the same place, because something about that spot is asking more than the steel can give. Welding the crack closed is only half of a good repair. The other half is understanding why it happened.

When a customer brings us a cracked bracket, a bent guard or a broken equipment mount, we look at where it failed, clean it back to bare steel, repair it, and talk about adding a gusset or rib so the next crack does not form. If the part is too far gone, we tell you and quote a new one instead.

Reinforcement that suits these parts

Not every part needs it. When one does, these are the options we usually discuss for steel parts repair.

How the job moves through the shop

  1. Look at the failure

    We look at where and how the part broke and ask how it is used.

  2. Clean and prepare

    Paint, rust and old weld are removed back to sound steel, and cracks are ground out.

  3. Repair and reinforce

    The part is welded, straightened if needed, and reinforced where we agreed.

  4. Finish and return

    Welds are cleaned up, edges broken, and the part is ready for paint and pickup.

Parts we often make this way

  • Motor and pump mounts
  • Machine guards and doors
  • Brackets on conveyors and racks
  • Equipment frames and stands
  • Steel trays and bins
  • Fixture plates and jigs

Repair or replace?

Repair makes sense when the part is mostly sound, hard to replace or needed back quickly. Replacement makes more sense when the steel is thin from rust, the part has been repaired many times, or a better design would solve the problem for good.

We look at the part with you and give you both options when both are reasonable.

What to bring

Bring the broken part, all of its pieces if it came apart, and if you can, a photo of where it was mounted. A note about how long it lasted and what it was doing when it failed helps us choose the right fix.

Clean parts are quicker to look at, but we can work with greasy or painted parts too.

Steel parts repair questions answered

How do we get the part to you?

Remove the part from the equipment and bring it to the shop during business hours. We call when it is ready for pickup.

Can you add a gusset during the repair?

Yes, and it is often the most useful part of the repair. We show you where it would go before we weld it.

How do we know if a part is worth repairing?

Bring it in or send photos. We tell you whether repair or a new part makes more sense and quote both if needed.

Do you repair stainless parts?

Yes. Stainless steel guards, trays and covers can be repaired with TIG welding.

Quote steel parts repair for your part

Send the drawing, sketch or sample with the quantity and material. We review it and reply with questions or a written quote.